اليكم تركيبة تصنيع منظف السطوح الصلبة
Part Ingredients Wt.%
A HOSTAPUR SAS 60 4.50
A GENAPOL UD-030 5.40
B Water (40-
A GENAPOL UD-030 5.40
B Water (40-
آ 50 °C) 39.80
C Preservative 0.10
C Perfume 0.20
D CALIBRITE SL 50.00
C Preservative 0.10
C Perfume 0.20
D CALIBRITE SL 50.00
Comments:
Tests:
Viscosity (mPas): 6400 (Brookfield RVT)
pH: 10.00
Manufacturing:
I One after another, the components of A are added to B.
II At آ 30 °C the components of C are added to I.
III At last, stir D to II.
Abrasive powders, based on silicium dioxyde are not common any
longer. Modern liquid products are based on calcium carbonate.
Viscosity (mPas): 6400 (Brookfield RVT)
pH: 10.00
Manufacturing:
I One after another, the components of A are added to B.
II At آ 30 °C the components of C are added to I.
III At last, stir D to II.
Abrasive powders, based on silicium dioxyde are not common any